[an error occurred while processing this directive]
综述:钢中亚稳奥氏体组织与疲劳性能关系
徐伟(),黄明浩,王金亮,沈春光,张天宇,王晨充
Review: Relations Between Metastable Austenite and Fatigue Behavior of Steels
XU Wei(),HUANG Minghao,WANG Jinliang,SHEN Chunguang,ZHANG Tianyu,WANG Chenchong

图9. 不同经验公式下奥氏体的堆垛层错能(γSF)、30%应变条件下50%奥氏体转变为马氏体的温度(Md30)与低周疲劳寿命Pearson相关性系数(ρXY)的关系

Fig.9. Relationships between ρXY of low cycle fatigue life and γSF and Md30 of austenite under different empirical equations distinguished by subscripts a~d (ρXY—Pearson correlation coefficient, γSF—stacking fault energy, Md30—temperature of 50% austenite transformed to martensite under 30% strain)