汽车用先进高强钢的氢脆研究进展
李金许(),王伟,周耀,刘神光,付豪,王正,阚博
A Review of Research Status of Hydrogen Embrittlement for Automotive Advanced High-Strength Steels
LI Jinxu(),WANG Wei,ZHOU Yao,LIU Shenguang,FU Hao,WANG Zheng,KAN Bo

图8. Fe-7Mn-0.1C-0.5Si 冷轧和热轧中锰钢充氢前后应力-应变曲线和EBSD像[98]

Fig.8. Stress-strain curves (a) and EBSD maps (b) of cold-rolled and hot-rolled medium-manganese steels (HRA—hot-rolled and annealed, CRA—cold-rolled and annealed, HRAH—H-charged HRA, CRAH—H-charged CRA)[98]Color online