[an error occurred while processing this directive]
汽车用先进高强钢的氢脆研究进展
李金许(),王伟,周耀,刘神光,付豪,王正,阚博
A Review of Research Status of Hydrogen Embrittlement for Automotive Advanced High-Strength Steels
LI Jinxu(),WANG Wei,ZHOU Yao,LIU Shenguang,FU Hao,WANG Zheng,KAN Bo

图6. Fe-0.22C-1.40Si-1.80Mn QP (淬火配分) 980钢在不同H含量下的工程应力-应变曲线[73]

Fig.6. Engineering stress-strain curves of QP980 steel with different hydrogen contents (RT—room temperature, QP—quenching & partitioning)[73]