热冲压成形钢的强度与塑性及断裂应变
|
|
Strength, Ductility and Fracture Strain ofPress-Hardening Steels
|
|
图16. Al-Si镀层热冲压零件涂装烘烤之后的弯曲载荷-位移曲线以及压溃后零件裂纹扩展情况 |
Fig.16. Bending load-displacement curves (a, b) and crack propagation after crushing (c~e) of Al-Si coated press hardening parts for the pre-coating thicknesses of 25 μm and 10 μm(a) hot stamped (b) hot stamped and baked (Crack extension of the hot stamped and baked parts by crush)(c) 14 d after crushing (10 μm) (d) 14 d after crushing (25 μm) (e) brittle fracture morphology (25 μm) |
![]() |