热冲压成形钢的强度与塑性及断裂应变
易红亮1,2(),常智渊1,才贺龙1,杜鹏举1,杨达朋1
Strength, Ductility and Fracture Strain ofPress-Hardening Steels
YI Hongliang1,2(),CHANG Zhiyuan1,CAI Helong1,DU Pengju1,YANG Dapeng1
图8. 淬火-闪配分(Q&FP)热冲压钢的TEM像
Fig.8. Bright-field (a, c) and dark-field (b, d) TEM images of the press-hardening steels QFP1500[21] (a, b) and QFP1800 (c, d) designed by Q&FP concept (γ presents retained austenite and the insets in Figs.8b and d show the SAED patterns of γ)