新型含Cu管线钢——提高管线耐微生物腐蚀性能的新途径 |
||||||||||||
| 杨柯,史显波,严伟,曾云鹏,单以银,任毅 | ||||||||||||
|
Novel Cu-Bearing Pipeline Steels: A New Strategy to Improve Resistance to Microbiologically Influenced Corrosion for Pipeline Steels |
||||||||||||
| Ke YANG,Xianbo SHI,Wei YAN,Yunpeng ZENG,Yiyin SHAN,Yi REN | ||||||||||||
| 表2 X80-Cu和X80钢在含有SRB的土壤浸出液中浸泡20 d后的点蚀坑数据统计 | ||||||||||||
| Table 2 Pit densities and depths on X80-Cu and X80 steels after 20 d immersion in the soil-extract solution | ||||||||||||
|
||||||||||||