新型含Cu管线钢——提高管线耐微生物腐蚀性能的新途径
杨柯1,史显波1,2(),严伟1,2,曾云鹏1,单以银1,2,任毅3,4
Novel Cu-Bearing Pipeline Steels: A New Strategy to Improve Resistance to Microbiologically Influenced Corrosion for Pipeline Steels
YANG Ke1,SHI Xianbo1,2(),YAN Wei1,2,ZENG Yunpeng1,SHAN Yiyin1,2,REN Yi3,4

图12. X80-Cu (A1.0Cu)和X80钢在铜绿假单胞菌(P. aeruginosa)菌液中经过1、3和5 d浸泡后的生物膜厚度[60]

Fig.12. Biofilm thicknesses on X80-Cu (A1.0Cu) and X80 steels after exposure to P. aeruginosa suspension for 1, 3 and 5 d[60]