[an error occurred while processing this directive]
新型含Cu管线钢——提高管线耐微生物腐蚀性能的新途径
杨柯1,史显波1,2(),严伟1,2,曾云鹏1,单以银1,2,任毅3,4
Novel Cu-Bearing Pipeline Steels: A New Strategy to Improve Resistance to Microbiologically Influenced Corrosion for Pipeline Steels
YANG Ke1,SHI Xianbo1,2(),YAN Wei1,2,ZENG Yunpeng1,SHAN Yiyin1,2,REN Yi3,4

图11. X80-Cu和X80钢在含有SRB的土壤浸出液中浸泡20 d后的点蚀坑三维形貌[63]

Fig.11. 3D images of the largest pits on X80-Cu (a) and X80 (b) steels after 20 d immersion in soil-extract solution with SRB[63]Color online