新型含Cu管线钢——提高管线耐微生物腐蚀性能的新途径
杨柯1,史显波1,2(),严伟1,2,曾云鹏1,单以银1,2,任毅3,4
Novel Cu-Bearing Pipeline Steels: A New Strategy to Improve Resistance to Microbiologically Influenced Corrosion for Pipeline Steels
YANG Ke1,SHI Xianbo1,2(),YAN Wei1,2,ZENG Yunpeng1,SHAN Yiyin1,2,REN Yi3,4

图9. X80-Cu钢和X80钢在含有SRB的土壤浸出液中浸泡20 d后表面腐蚀形貌的SEM像[63]

Fig.9. Surface SEM images of X80-Cu (a) and X80 (b) steels immersed in soil-extract solution with SRB for 20 d, after removal of the corrosion products[63]