图4. 不同激光扫描速率下熔池尺寸的数值模拟与实验结果对比

Fig.4. Comparisons of simulation and experimental results of the molten pool width and depth at the cross-section under different laser scan rates (Insets show the OM images of molten pools under scanning velocities of 500, 700 and 1000 mm/s, respectively)