考虑塑性变形和相变耦合效应的NiTiNb记忆合金管接头装配性能模拟
陈翔1,2,3,陈伟1,赵洋1,禄盛1,3,金晓清2,彭向和2()
Assembly Performance Simulation of NiTiNb Shape Memory Alloy Pipe Joint Considering Coupling Effect of Phase Transformation and Plastic Deformation
CHEN Xiang1,2,3,CHEN Wei1,ZHAO Yang1,LU Sheng1,3,JIN Xiaoqing2,PENG Xianghe2()

图8. 不同h下NiTiNb SMA管接头内表面接触压力云图

Fig.8. Contact pressure distributions of inner surface of NiTiNb SMA joint with h=0.14 mm (a), h=0.15 mm (b), h=0.16 mm (c), h=0.17 mm (d), h=0.18 mm (e), h=0.19 mm (f), h=0.20 mm (g) and h=0.21mm (h)Color online