新型多层金属复合材料的制备与性能
|
|
Fabrication and Properties of Novel Multi-LayeredMetal Composites
|
|
图12. 9层和11层金属复合材料在不同状态下的三点弯曲侧面断口形貌的SEM像 |
Fig.12. Side fracture SEM images of three-point bending of 9 layered (a~c) and 11 layered (d~f) composites(a, d) CR (b, e) CR+S (c, f) CR+S+A |
![]() |