新型多层金属复合材料的制备与性能
|
|
Fabrication and Properties of Novel Multi-LayeredMetal Composites
|
|
图7. 真空热压后不同层数的块体MAS/316L不锈钢多层复合材料照片 |
Fig.7. Photos of bulk multi-layered MAS/316L stainless steel composites with different layers after hot pressing in vacuum(a) 9 layers (b) 11 layers |
![]() |