新型多层金属复合材料的制备与性能
|
|
Fabrication and Properties of Novel Multi-LayeredMetal Composites
|
|
图2. 不同变形量时金属复合材料的界面特征 |
Fig.2. Interface characteristics of metal composites under different deformation reductions(a) 10% (b) 20% (c) 40% (d) 60% (e) 80% (f) enlarged view of square area in Fig.2b |
![]() |