新型多层金属复合材料的制备与性能
|
|
Fabrication and Properties of Novel Multi-LayeredMetal Composites
|
|
图1. 异质母材界面结合、拉伸取样及块体多层复合材料示意图 |
Fig.1. Schematic of interface bonding (a), sampling method for tensile tests of heterogeneous initial material (b) and bulk multilayered composite (c) |
![]() |