图5. CoCrFeNiMo0.2高熵合金的初始试样、RTR35%和CTR35%试样及其经800 ℃、30 min退火处理试样的拉伸应力-应变曲线与加工硬化速率曲线

Fig.5. Engineering stress-engineering strain curves (a) and work hardening rate curves (b) of CoCrFeNiMo0.2 high-entropy alloy samples of initial condition, RTR35%, CTR35% and their heat treated samplesColor online