Nb对Fe22Cr5Al3Mo合金显微组织和耐腐蚀性能的影响
钱月,孙蓉蓉,张文怀,姚美意,张金龙,周邦新,仇云龙,杨健,成国光,董建新

Effect of Nb on Microstructure and Corrosion Resistance of Fe22Cr5Al3Mo Alloy
Yue QIAN,Rongrong SUN,Wenhuai ZHANG,Meiyi YAO,Jinlong ZHANG,Bangxin ZHOU,Yunlong QIU,Jian YANG,Guoguang CHENG,Jianxin DONG
表3 Fe22Cr5Al3Mo-xNb合金中几种典型第二相尺寸统计 (nm)
Table 3 Size statistics of the typical SPPs in Fe22Cr5Al3Mo-xNb alloys (nm)
Alloyhcp-Fe2Nbhcp-Cr2Nbfcc-Cr23C6o-Fe3Cfcc-Nb(C, N)
0Nb--500~800200-
0.5Nb150~200About 500--About 190
1.0Nb150~800500~750--About 185
2.0Nb300~2000500~800--About 170