表2 Fe22Cr5Al3Mo-xNb合金的XRD特征峰参数(θ,d)和晶格常数平均值(ā)
Table 2 XRD characteristic peak parameters (θ, d) and average lattice constant (ā) of Fe22Cr5Al3Mo-xNb alloy
Alloy(110)(200)(211)ā / nm
θ / (°)d / nmθ / (°)d / nmθ / (°)d / nm
0Nb44.480.2035264.790.1437782.190.117190.28747
0.5Nb44.450.2036564.790.1437782.130.117250.28758
1.0Nb44.450.2036564.580.1441982.130.117250.28786
2.0Nb44.240.2045664.310.1447381.410.118110.28935