Nb对Fe22Cr5Al3Mo合金显微组织和耐腐蚀性能的影响
钱月,孙蓉蓉,张文怀,姚美意,张金龙,周邦新,仇云龙,杨健,成国光,董建新

Effect of Nb on Microstructure and Corrosion Resistance of Fe22Cr5Al3Mo Alloy
Yue QIAN,Rongrong SUN,Wenhuai ZHANG,Meiyi YAO,Jinlong ZHANG,Bangxin ZHOU,Yunlong QIU,Jian YANG,Guoguang CHENG,Jianxin DONG
表1 Fe22Cr5Al3Mo-xNb合金的成分 (mass fraction / %)
Table 1 Chemical compositions of the Fe22Cr5Al3Mo-xNb alloys (mass fraction / %)
AlloyCrAlMoNbCNFe
0Nb22.905.253.640.030.0320.0089Bal.
0.5Nb22.455.173.520.470.0250.0047Bal.
1.0Nb22.895.293.730.980.0220.0039Bal.
2.0Nb23.395.373.841.960.0360.0082Bal.