[an error occurred while processing this directive]
Nb对Fe22Cr5Al3Mo合金显微组织和耐腐蚀性能的影响
钱月1,孙蓉蓉1,张文怀1,姚美意1(),张金龙1,周邦新1,仇云龙2,杨健3,成国光4,董建新5
Effect of Nb on Microstructure and Corrosion Resistance of Fe22Cr5Al3Mo Alloy
QIAN Yue1,SUN Rongrong1,ZHANG Wenhuai1,YAO Meiyi1(),ZHANG Jinlong1,ZHOU Bangxin1,QIU Yunlong2,YANG Jian3,CHENG Guoguang4,DONG Jianxin5

图3. Fe22Cr5Al3Mo-xNb合金中典型第二相粒子的TEM明场像、SAED花样和EDS结果

Fig.3. TEM bright field images of the second phase particles (SPPs) of 0.5Nb (a1), 0Nb (a2, a3), 1.0Nb (a4) and 2.0Nb (a5, a6), and SAED patterns (b1~b5) and EDS results (c1~c5) corresponding to the P1~P5 typical SPPs respectively in Fe22Cr5Al3Mo-xNb alloys