Nb对Fe22Cr5Al3Mo合金显微组织和耐腐蚀性能的影响
钱月1,孙蓉蓉1,张文怀1,姚美意1(),张金龙1,周邦新1,仇云龙2,杨健3,成国光4,董建新5
Effect of Nb on Microstructure and Corrosion Resistance of Fe22Cr5Al3Mo Alloy
QIAN Yue1,SUN Rongrong1,ZHANG Wenhuai1,YAO Meiyi1(),ZHANG Jinlong1,ZHOU Bangxin1,QIU Yunlong2,YANG Jian3,CHENG Guoguang4,DONG Jianxin5

图1. Fe22Cr5Al3Mo-xNb合金的XRD谱

Fig.1. XRD spectra of Fe22Cr5Al3Mo-xNb alloys