高温合金单晶铸件中条纹晶的形成机制
马德新1,2,王富3,徐维台1,徐文梁3,赵运兴1()
Formation of Sliver Defects in Single CrystalCastings of Superalloys
MA Dexin1,2,WANG Fu3,XU Weitai1,XU Wenliang3,ZHAO Yunxing1()

图9. 枝晶横向收缩(包括法向和切向收缩)引起的条纹晶产生机制示意图

Fig.9. Schematic of sliver formation caused by lateral shrinkage force in normal (FN) and tangential direction (FT)(a) dendrite growth into mold hole (b) rotation of the broken dendrite