高温合金单晶铸件中条纹晶的形成机制
马德新1,2,王富3,徐维台1,徐文梁3,赵运兴1()
Formation of Sliver Defects in Single CrystalCastings of Superalloys
MA Dexin1,2,WANG Fu3,XU Weitai1,XU Wenliang3,ZHAO Yunxing1()

图6. 图5e中试样截面的EDS扫描结果

Fig.6. EDS mapping analyse on the specimen section showing in Fig.5eColor online(a) Al (b) O (c) Ni (d) Ti (e) W (f) Re