高温合金单晶铸件中条纹晶的形成机制
马德新1,2,王富3,徐维台1,徐文梁3,赵运兴1()
Formation of Sliver Defects in Single CrystalCastings of Superalloys
MA Dexin1,2,WANG Fu3,XU Weitai1,XU Wenliang3,ZHAO Yunxing1()

图3. 另一例条纹晶缺陷及起源处的放大OM像

Fig.3. OM image of sliver defect in another example (a) and the magnification of its origin (b)