部分再结晶退火对无取向硅钢的磁性能与力学性能的影响
于雷,罗海文()
Effect of Partial Recrystallization Annealing on Magnetic Properties and Mechanical Properties of Non-Oriented Silicon Steel
YU Lei,LUO Haiwen()

图6. 不同工艺退火后含Nb无取向硅钢冷轧后的织构组

Fig.6. α-fiber (a) and γ-fiber (b) texture components in Nb-containing non-oriented silicon steel after cold rolling and the different annealing processes (f(g)—orientation distribution function, g= (φ1, Φ, φ2))