Si对铸造超高铬高碳双相钢组织及性能的影响
王桂芹,王琴,车宏龙,李亚军,雷明凯()
Effects of Silicon on the Microstructure and Propertiesof Cast Duplex Stainless Steel with Ultra-HighChromium and High Carbon
WANG Guiqin,WANG Qin,CHE Honglong,LI Yajun,LEI Mingkai()

图14. 超高铬高碳钢固溶处理试样在硼酸溶液中自钝化膜的Mott-Schottky曲线

Fig.14. Mott-Schottky plots of the passive films formed on ultra-high chromium and high carbon steel in boric acid solution after solution treatment (C—capacitance of electronic double-layer)