[an error occurred while processing this directive]
Si对铸造超高铬高碳双相钢组织及性能的影响
王桂芹,王琴,车宏龙,李亚军,雷明凯()
Effects of Silicon on the Microstructure and Propertiesof Cast Duplex Stainless Steel with Ultra-HighChromium and High Carbon
WANG Guiqin,WANG Qin,CHE Honglong,LI Yajun,LEI Mingkai()

图10. 超高铬高碳钢固溶处理试样的拉伸断口形貌

Fig.10. Tensile fracture morphologies of ultra-high chromium and high carbon steel with 0.46%Si (a) and 1.36%Si (b) after solution treatment