Si对铸造超高铬高碳双相钢组织及性能的影响
王桂芹,王琴,车宏龙,李亚军,雷明凯()
Effects of Silicon on the Microstructure and Propertiesof Cast Duplex Stainless Steel with Ultra-HighChromium and High Carbon
WANG Guiqin,WANG Qin,CHE Honglong,LI Yajun,LEI Mingkai()

图4. 超高铬高碳钢铸态试样的背散射电子像

Fig.4. Backscattered electron images of as-cast ultra-high chromium and high carbon steel(a) full view of 0.46%Si (b) eutectoid structure in the core of area A of 0.46%Si(c) full view of 1.36%Si (d) eutectoid structure in the core of area A of 1.36%Si