脉冲电流调控金属熔体中的非金属夹杂物
张新房(),闫龙格
Regulating the Non-Metallic Inclusions by Pulsed Electric Current in Molten Metal
ZHANG Xinfang(),YAN Longge

图26. 不同类型电流去除夹杂物效率[34,49,54,56,57,58,68,69]

Fig.26. Inclusion removal efficiency of different current types[34,49,54,56,57,58,68,69]