脉冲电流调控金属熔体中的非金属夹杂物
张新房(),闫龙格
Regulating the Non-Metallic Inclusions by Pulsed Electric Current in Molten Metal
ZHANG Xinfang(),YAN Longge

图14. 脉冲电流处理前后试样中部MgO夹杂物尺寸分布

Fig.14. Particle size distributions of MgO inclusions on the middle part of the sample before and after electric pulse treatment