脉冲电流调控金属熔体中的非金属夹杂物
张新房(),闫龙格
Regulating the Non-Metallic Inclusions by Pulsed Electric Current in Molten Metal
ZHANG Xinfang(),YAN Longge

图7. 电熔剂精炼工艺原理图