石墨烯纳米片增强镁基复合材料力学性能及增强机制
周霞1,2(),刘霄霞2
Mechanical Properties and Strengthening Mechanism of Graphene Nanoplatelets Reinforced Magnesium Matrix Composites
ZHOU Xia1,2(),LIU Xiaoxia2

图9. 复合材料中未包Ni和包覆Ni的GNP的拉伸变形演化过程

Fig.9. MD snapshots of lattice configuration variation of uncoated-Ni GNP (GNP) (a~c) and double side Ni-coated GNP (Ni-GNP-Ni) (d~f) in the GNP/Mg composite during tensile process(a) ε=0.188 (b) ε=0.189 (c) ε=0.19 (d) ε=0.186 (e) ε=0.187 (f) ε=0.188