[an error occurred while processing this directive]
石墨烯纳米片增强镁基复合材料力学性能及增强机制
周霞1,2(),刘霄霞2
Mechanical Properties and Strengthening Mechanism of Graphene Nanoplatelets Reinforced Magnesium Matrix Composites
ZHOU Xia1,2(),LIU Xiaoxia2

图6. 不同层数的GNPs/Mg复合材料的拉伸应力-应变曲线

Fig.6. Tensile stress-strain curves of GNPs/Mg nanocomposites with different layers of GNP