表2 普碳钢Q235和6061铝合金的力学性能
Table 2 Mechanical properties of the used materials in the experiment

Material

Ultimate tensile strength

MPa

Yield strength

MPa

Shear strength

MPa

Fracture elongation

%

Q235351±5235±4197±436.5±1.5
6061215±4141±3124±324.7±0.8