[an error occurred while processing this directive]
Zr-0.75Sn-0.35Fe-0.15Cr合金在250 ℃去离子水中的初期腐蚀行为
姚美意1,2(),张兴旺1,2,侯可可1,2,张金龙1,2,胡鹏飞1,2,彭剑超1,2,周邦新1,2
The Initial Corrosion Behavior of Zr-0.75Sn-0.35Fe-0.15Cr Alloy in Deionized Water at 250 ℃
YAO Meiyi1,2(),ZHANG Xingwang1,2,HOU Keke1,2,ZHANG Jinlong1,2,HU Pengfei1,2,PENG Jianchao1,2,ZHOU Bangxin1,2

图4. 图2i中点9的TEM像、SAED花样、HRTEM像和FFT图

Fig.4. TEM image (a), SAED pattern of square area in Fig.4a (b), HRTEM image (c) and FFT image of square area in Fig.4c (d) of point 9 in Fig.2i