Zr-0.75Sn-0.35Fe-0.15Cr合金在250 ℃去离子水中的初期腐蚀行为
姚美意1,2(),张兴旺1,2,侯可可1,2,张金龙1,2,胡鹏飞1,2,彭剑超1,2,周邦新1,2
The Initial Corrosion Behavior of Zr-0.75Sn-0.35Fe-0.15Cr Alloy in Deionized Water at 250 ℃
YAO Meiyi1,2(),ZHANG Xingwang1,2,HOU Keke1,2,ZHANG Jinlong1,2,HU Pengfei1,2,PENG Jianchao1,2,ZHOU Bangxin1,2

图3. 分别对应图2a~i中点1~9的SAED花样

Fig.3. SAED patterns corresponding to points 1~9 in Figs.2a~i (a~i), respectively