[an error occurred while processing this directive]
Ag-Ni偏晶合金凝固过程研究
邓聪坤1,2,江鸿翔1,赵九洲1(),何杰1,赵雷3
Study on the Solidification of Ag-Ni Monotectic Alloy
DENG Congkun1,2,JIANG Hongxiang1,ZHAO Jiuzhou1(),HE Jie1,ZHAO Lei3

图11. 不同成分Ag-Ni合金凝固组织中富Ni相粒子平均半径(<R>)随富Ni相液滴/粒子T.nuc的变化

Fig.11. Experimental results (solid circles) and calculated results (open circles) of the average radius (<R>) of the Ni-rich particles in Ag-xNi alloys with x=1.25% (blue color), x=2.24% (green color), x=3.0% (red color), x=4.0% (black color) vsT.nuc of the Ni-rich droplets/particles