| Thermal conductivity of liquid Ag | 122.29093+0.04259T | W·K-1·m-1 |
| Thermal conductivity of liquid Ni | 57 | W·K-1·m-1 |
| Thermal conductivity of solid Ag | 429 | W·K-1·m-1 |
| Thermal conductivity of solid Ni | 90.7 | W·K-1·m-1 |
| Density of liquid Ag | 9330-0.91(T-1233.7) | kg·m-3 |
| Density of liquid Ni | 7905-1.19(T-1727) | kg·m-3 |
| Density of solid Ag | 10500 | kg·m-3 |
| Density of solid Ni | 8900 | kg·m-3 |
| Specific heat of liquid Ag | 283 | J·kg-1·K-1 |
| Specific heat of liquid Ni | 620 | J·kg-1·K-1 |
| Specific heat of solid Ag | 235 | J·kg-1·K-1 |
| Specific heat of solid Ni | 444 | J·kg-1·K-1 |
| Latent heat of solidification of pure Ag | 102809 | J·kg-1 |
| Latent heat of solidification of pure Ni | 292334 | J·kg-1 |