[an error occurred while processing this directive]
Ag-Ni偏晶合金凝固过程研究
邓聪坤1,2,江鸿翔1,赵九洲1(),何杰1,赵雷3
Study on the Solidification of Ag-Ni Monotectic Alloy
DENG Congkun1,2,JIANG Hongxiang1,ZHAO Jiuzhou1(),HE Jie1,ZHAO Lei3

图7. Ag-4.0%Ni合金中富Ni相粒子<R>2D和富Ni相液滴形核阶段熔体冷却速率(T.nuc)随试样直径的变化

Fig.7. Experimental results (black symbols) and calculated results (black line) of <R>2D of the Ni-rich particles in Ag-4.0%Ni alloys and the cooling rate of the melt during the nucleation (T.nuc, red line and symbols) of the Ni-rich droplets as a function of sample diameter