Ag-Ni偏晶合金凝固过程研究
邓聪坤1,2,江鸿翔1,赵九洲1(),何杰1,赵雷3
Study on the Solidification of Ag-Ni Monotectic Alloy
DENG Congkun1,2,JIANG Hongxiang1,ZHAO Jiuzhou1(),HE Jie1,ZHAO Lei3

图5. Ag-Ni合金中富Ni相粒子二维平均半径(<R>2D)随合金成分的变化

Fig.5. Average 2D radius (<R>2D) of the Ni-rich particles in Ag-Ni alloys for the samples of 5 mm in diameter vs alloy composition