[an error occurred while processing this directive]
Ag-Ni偏晶合金凝固过程研究
邓聪坤1,2,江鸿翔1,赵九洲1(),何杰1,赵雷3
Study on the Solidification of Ag-Ni Monotectic Alloy
DENG Congkun1,2,JIANG Hongxiang1,ZHAO Jiuzhou1(),HE Jie1,ZHAO Lei3

图2. 直径为8 mm的Ag-4.0%Ni合金中富Ni相粒子分布示意图及实测富Ni相粒子体积分数(φsβ)沿试样轴向和径向分布

Fig.2. Schematic distribution of the Ni-rich particles in Ag-4.0%Ni alloy with a diameter of 8 mm (a), measured volume fraction (φsβ) distributions of the Ni-rich particles along the axial z direction (b) and radial r direction (c)