Ag-Ni偏晶合金凝固过程研究
邓聪坤1,2,江鸿翔1,赵九洲1(),何杰1,赵雷3
Study on the Solidification of Ag-Ni Monotectic Alloy
DENG Congkun1,2,JIANG Hongxiang1,ZHAO Jiuzhou1(),HE Jie1,ZHAO Lei3

图1. 不同直径(d) Ag-4.0%Ni合金试样心部的冷却曲线

Fig.1. Experimental results (symbols) and calculated results (solid lines) of the cooling curves for the center region of Ag-4.0%Ni alloys with different diameters (d) (T—temperature, t—time, Tm and Te refer to the monotectic reaction temperature and the eutectic reaction temperature of Ag-Ni alloy, respectively)