[an error occurred while processing this directive]
TA32钛合金厚板的微观组织、织构与力学性能
程超1,2,陈志勇1,2(),秦绪山3,刘建荣1,2,王清江1,2
Microstructure, Texture and Mechanical Property ofTA32 Titanium Alloy Thick Plate
CHENG Chao1,2,CHEN Zhiyong1,2(),QIN Xushan3,LIU Jianrong1,2,WANG Qingjiang1,2

图13. 热处理后板材厚度截面上不同位置的(0002)极图分布

Fig.13. The (0002) PF distributions of TA32 thick plate after heat treatment