[an error occurred while processing this directive]
TA32钛合金厚板的微观组织、织构与力学性能
程超1,2,陈志勇1,2(),秦绪山3,刘建荣1,2,王清江1,2
Microstructure, Texture and Mechanical Property ofTA32 Titanium Alloy Thick Plate
CHENG Chao1,2,CHEN Zhiyong1,2(),QIN Xushan3,LIU Jianrong1,2,WANG Qingjiang1,2

图11. TA32钛合金厚板表层及中心厚度处的局部取向差(LM)分析结果

Fig.11. Local misorientation (LM) results of TA32 titanium alloy thick plate at the surface (a) and 1/2 thickness (b) (Insets show the volume fraction distributions of LM)