TA32钛合金厚板的微观组织、织构与力学性能
程超1,2,陈志勇1,2(),秦绪山3,刘建荣1,2,王清江1,2
Microstructure, Texture and Mechanical Property ofTA32 Titanium Alloy Thick Plate
CHENG Chao1,2,CHEN Zhiyong1,2(),QIN Xushan3,LIU Jianrong1,2,WANG Qingjiang1,2

图10. TA32钛合金厚板表层及中心厚度处的极图及Schmidt因子分布

Fig.10. PF maps (a, d) and Schmidt factor maps (b, c, e, f) at the surface (a~c) and 1/2 thickness (d~f) (Insets in Figs.10b, c, e and f show the volume fraction distributions of SF)