TA32钛合金厚板的微观组织、织构与力学性能
程超1,2,陈志勇1,2(),秦绪山3,刘建荣1,2,王清江1,2
Microstructure, Texture and Mechanical Property ofTA32 Titanium Alloy Thick Plate
CHENG Chao1,2,CHEN Zhiyong1,2(),QIN Xushan3,LIU Jianrong1,2,WANG Qingjiang1,2

图9. 柱面<a>滑移和基面<a>滑移的施密特Schmidt因子分布和c轴与加载方向夹角(θ)之间的关系

Fig.9. Schmidt factor (SF) distribution of two slip systems (prismatic and basal <a> slips) as a function of θ (θ—angle between c-axis and loading axis)