表2 GH4720Li合金二级均匀化热处理实验方案
Table 2 Two-stage homogenization heat treatment (TSHT) schedules for the GH4720Li alloy
No.Two stage heat treatment
TSHT 11130 ℃, 8 h+1160 ℃, 4 h, WC
TSHT 21130 ℃, 16 h+1160 ℃, 8 h, WC
TSHT 31160 ℃, 8 h+1180 ℃, 2 h, WC
TSHT 41140 ℃, 12 h+1170 ℃, 10 h, AC