热处理工艺对GH4720Li合金细晶铸锭组织与热加工性能的影响
王涛,万志鹏,李钊,李佩桓,李鑫旭,韦康,张勇

Effect of Heat Treatment Parameters on Microstructure and Hot Workability of As-Cast Fine Grain Ingot of GH4720Li Alloy
Tao WANG,Zhipeng WAN,Zhao LI,Peihuan LI,Xinxu LI,Kang WEI,Yong ZHANG
表1 GH4720Li合金一级均匀化热处理实验方案
Table 1 One-stage homogenization heat treatment (OSHT) schedules for the GH4720Li alloy
No.One stage heat treatment
OSHT 11140 ℃, 1 h, WC
OSHT 21140 ℃, 8 h, WC
OSHT 31140 ℃, 16 h, WC
OSHT 41160 ℃, 1 h, WC
OSHT 51160 ℃, 14 h, WC
OSHT 61160 ℃, 24 h, AC
OSHT 71160 ℃, 14 h, 0.2 ℃·min-1 FC to 1010 ℃, and then AC