取向偏差对镍基单晶高温合金钎焊接头组织与力学性能的影响
赵旭1,2,孙元2(),侯星宇2,张洪宇2,周亦胄1,2(),丁雨田1
Effect of Orientation Deviation on Microstructure and Mechanical Properties of Nickel-Based Single Crystal Superalloy Brazing Joints
ZHAO Xu1,2,SUN Yuan2(),HOU Xingyu2,ZHANG Hongyu2,ZHOU Yizhou1,2(),DING Yutian1

图9. 取向差钎焊接头形成机理与热处理过程示意图

Fig.9. Schematics of formation mechanism and heat treatment process of brazed joint with orientation deviation(a) heating (b) holding (c) brazing joint (d) heat treatment joint