[an error occurred while processing this directive]
取向偏差对镍基单晶高温合金钎焊接头组织与力学性能的影响
赵旭1,2,孙元2(),侯星宇2,张洪宇2,周亦胄1,2(),丁雨田1
Effect of Orientation Deviation on Microstructure and Mechanical Properties of Nickel-Based Single Crystal Superalloy Brazing Joints
ZHAO Xu1,2,SUN Yuan2(),HOU Xingyu2,ZHANG Hongyu2,ZHOU Yizhou1,2(),DING Yutian1

图1. 钎焊连接试样示意图

Fig.1. Schematic of specimen for brazed bonding (The axial direction of the specimen 1 is parallel to [001] and specimen 2 is deviated from [001] by θ angle; θ=0°, 45° and 90°, respectively)